he found that printing ABS parts on top of a thin layer of PLA has proven a great way to improve bed adhesion and reduce warping. He’s extended this technique further to other material ...
Baking the PLA at 100°C for 30 minutes generally improves material properties, but also can cause warping and shrinking. The effective warping and shrinking differed wildly between the filament.
These adjustments not only enhance the natural texture of wooden PLA but also reduce common issues such as stringing, warping, and uneven extrusion. Fine-tuning your slicer settings is a critical ...